Usage

for integration in standard microscope eyepieces

Article

Crosshair Eyepiece Graticules positive

  • Material: B270
  • Substrate thickness: 1,5mm
  • Structure: opaque crosshair on transparent background
    • Chrome HRC: OD > 3, reflection ca. 45%, @550nm
  • AR-Coating: none
POSITIVE graticule diameter in mm
line thickness ø 26.5 h8 ø 26.0 h8 ø 21.0 h8 ø 19.0 h8
in mm Item No. Item No. Item No. Item No.
0.005 10008.03.101 10008.03.105 10008.03.109 10008.03.097
0.010 10008.03.102 10008.03.106 10008.03.110 10008.03.098
0.020 10008.03.103 10008.03.107 10008.03.111 10008.03.099
0.030 10008.03.104 10008.03.108 10008.03.112 10008.03.100

Article

Crosshair Eyepiece Graticules negative

  • Material: B270
  • Substrate thickness: 1,5mm
  • Structure: opaque crosshair on transparent background
    • Chrome HRC: OD > 4, reflection < 15%, @550nm
  • AR-Coating: none
NEGATIVE graticule diameter in mm
line thickness ø 26.5 h8 ø 26.0 h8 ø 21.0 h8 ø 19.0 h8
in mm Item No. Item No. Item No. Item No.
0.005 10008.03.201 10008.03.205 10008.03.209 10008.03.197
0.010 10008.03.202 10008.03.206 10008.03.210 10008.03.198
0.020 10008.03.203 10008.03.207 10008.03.211 10008.03.199
0.030 10008.03.204 10008.03.208 10008.03.212 10008.03.200

Get expert advice

Sales Germany

Andreas Franke


Sales International

USA & Canada

POG Precision Optics Gera Corp.

Buzz Nesti, President

Glen Dunn, Sales Manager

Phone
Fax

Israel

Optics & Motion

Ruben Fainsod

Phone

www.opticsmotion.com