Glass Scale 150 mm

  • Material: Sodalime
  • Dimensions [mm]: 170 x 16 x 2.3
  • Structure: divisions in Chrom LRC
    • Chrom LRC: OD>3, Reflexion<15% @550nm
    • 150mm in 1500 divisionsdivision
    • Line thickness: 20µm
  • AR Coating: none
  • Certificate of conformity: on request

 

Type Item No.
Glass Scales 100 mm 10008.03.019
Variants with low thermal expansion
Implementation with Nextrema 712-3 (dark), thickness: 2.0 mm 10008.03.042
Implementation with Nextrema 724-3 (transparent), thickness: 2.0 mm 10008.03.043

 

Article

 

Glas scale 100 mm

  • Material: Sodalime
  • Dimensions [mm]: 120 x 16 x 2.3
  • Structure: Division in Chrom LRC
    • Chrom LRC, OD>3, Reflexion<15% @550nm
    • 100mm in 1000 divisions
    • Line width: 20µm
  • AR Coating: none
  • Certificate of conformity: on request
Type Item No.
Glass scale 100 mm 10008.03.019
Variants with low thermal expansion
Implementation with Nextrema 712-3 (dark), thickness: 2.3 mm 10008.03.042
Implementation with Nextrema 724-3 (transparent), thickness: 2.3 mm 10008.03.043

Article

 

Glas scale 150 mm

  • Material: Sodalime
  • Dimensions [mm]: 170 x 16 x 2.3
  • Struktur: Teilung in Chrom LRC
    • Chrom LRC: OD>3, Reflexion<15% @550nm
    • 150mm in 1500 divisions
    • Line width: 20µm
  • AR Coating: none
  • Certificate of conformity: on request
Type Item No.
Glass Scale 150 mm 10008.03.020

 

Get expert advice

Sales Germany

Andreas Franke


Sales International

USA & Canada

POG Precision Optics Gera Corp.

Buzz Nesti, President

Glen Dunn, Sales Manager

Phone
Fax

Israel

Optics & Motion

Ruben Fainsod

Phone

www.opticsmotion.com